Search
Use the search bar or filters below to find any TAPPI product or publication.
Filters
Content Type
Publications
Level of Knowledge
Committees
Collections
Journal articles
Alternative disposal methods for pulp mill biosludge
ABSTRACT: The chemical pulp production process produces notable amounts of biosludge, mostly in the wastewater treatment system. Biosludge is a problematic waste stream due to its properties, and recently, its amounts have been on the increase. The most used disposal processes are incineration in a bark boiler or a recovery boiler now that landfilling is no longer permitted by legislation in many countries. Incineration of wet sludges with poor drying characteristics decreases the energy efficiency of the process. Biosludge is typically mixed with black liquor in the evaporation plant before feeding to the recovery boiler. Although the recovery boiler is designed to handle challenging fuels, biosludge disposal requires consideration of its behavior during evaporation and accumulation of non-process elements in the recovery cycle. This study discusses the currently used sludge handling methods and presents two novel methods, hydrothermal carbonization and anaerobic digestion, to convert sludge into a usable form. Production of hydrochar or biogas offers new usage possibilities for biosludge and improves the energy efficiency of the mill when the new methods replace incineration. The processes are still developing, and thus their economic feasibility is uncertain; however, depending on the case details, they can be considered promising alternatives to be implemented in the future.
Journal articles
Effects of calcium on sodium salt scaling with the presence of resin acids and fatty acids, TAPPI Journal June 2026
ABSTRACT: Reintroducing tall oil soap or its related products into high dry solids black liquor has been found to reduce sodium salt scaling in falling film evaporators. Aside from resin acids and fatty acids, which are the likely scale inhibitors, calcium is reintroduced into black liquor because of the relatively high calcium content of tall oil soap. One concern is that this increase in calcium content might lead to the formation of additional calcium and sodium scales in evaporators. In this work, we investigated the relationship among trace amounts of calcium, sodium salts, resin acids, and fatty acids in a controlled system using a model salt solution and a benchtop setup. We studied the effects of the calcium carbonate addition and calcium carbonate scales on sodium salt scaling in the presence of resin acids and fatty acids. We found that some calcium carbonate is incorporated in the precipitated sodium crystals, and the suspended sodium crystals become larger and more compact with increasing calcium carbonate concentration. Experiments in the benchtop setup show that precipitating calcium carbonate scale on the heat exchanger does not lead to a higher rate of sodium salt scaling. The solubility of calcium carbonate is not affected by the addition of resin acids and fatty acids. These findings indicate that the reduction in sodium salt scaling through the addition of tall oil soap is primarily related to resin acids and fatty acids, rather than to calcium or to interactions between calcium and mixtures of resin and fatty acids.
Journal articles
Preparation of a vegan leather from mycelium with papermaking method, TAPPI Journal June 2026
ABSTRACT: With growing concern over the environmental impacts of both natural leather and conventional synthetic leathers, the development of sustainable and eco-friendly leather alternatives has become an urgent research priority. In this study, an innovative wet papermaking strategy is proposed to fabricate continuous, homogeneous mycelial sheets from chitin-rich fungal mycelium, mimicking the matrix structure of genuine leather. These mycelial sheets were chemically modified to meet the performance requirements of leather foam layers. Subsequently, the modified mycelial sheets were combined with a substrate fabric to produce a novel mycelium-based leather composite (myco-paper leather) that achieves an excellent balance of mechanical properties and tactile qualities. Experimental results demonstrate that the mycelium-sheet-based leather substitute exhibits remarkable mechanical performance, with a tensile strength of approximately 45 MPa and an elongation at break of about 10.5%. After lamination with the substrate fabric, the composite material shows a tear strength of approximately 16 N, along with a desirable hand feel and surface texture. Following tannic acid tanning, the mycelial sheets also exhibit significant antimicrobial and antifungal properties, forming an inhibition zone of approximately 2 mm against Staphylococcus aureus. Through reinforcement with plant fibers, the developed material attains both strength and flexibility, indicating that the wet papermaking of mycelial sheets is a feasible and scalable approach for producing sustainable leather alternatives. This work not only employs a simple and mature papermaking process to process fungal mycelium but also provides a new conceptual and practical foundation for the large-scale production of bio-based leather substitutes. The findings have significant implications for advancing a low-carbon, sustainable leather industry.
Journal articles
Investigation of the factors contributing to malodorous gases emission during secondary fiber reuse, TAPPI Journal June 2026
ABSTRACT: Malodorous gases are commonly produced during secondary fiber reuse, which is harmful to human health and causes environmental pollution. This paper investigated the influence of fiber type and concentration, temperature, and whitewater concentration on the malodorous gases. The results indicated that, in pulp prepared with fresh water, bleached hardwood kraft pulp (LBKP) did not produce malodorous gases after standing for five days. In contrast, the secondary fiber began to release substantial amounts of total volatile organic compounds (TVOC) on the third day and hydrogen sulfide (H2S) and ammonia (NH3) on the sixth day, and black substances began to appear in the pulp, which proved that the microorganisms began to proliferate. With the increase of the secondary fiber concentration, the release amounts of TVOC, H2S, and NH3 gradually rose, along with the black substances in the pulp. With increased temperature, the release of TVOC increased steadily, while the release of H2S and NH3 reached the maximum at about 45°C, and then began to decline. The decrease of the pulp freeness accelerated the generation of the malodorous gases, but the total release amounts of TVOC, H2S, and NH3 were basically the same. With the increase of white water concentration, the release of TVOC, H2S, and NH3 increased rapidly. When the white water/fresh water was 20 mL/80 mL, the slurry changed from pale yellow to aterrimus on the sixth day. Therefore, microorganisms in the secondary fiber caused pulp deterioration, while white water was the main reason for generating a large amount of malodorous gases.
Journal articles
Moisture performance of silica-paper hybrids in the hygroscopic range, TAPPI Journal March 2026
ABSTRACT: Vapor retarders, crucial in building constructions, are traditionally made from plastic-based materials, raising environmental concerns due to the use of fossil materials. This study explores the potential of functionalized papers, particularly silica-paper hybrids, as sustainable alternatives. This work delves into the moisture properties of sol-gel coated linter papers, considering the water vapor permeability and physisorption behavior following DIN EN ISO 12572 and DIN EN ISO 12571. The study addresses hysteresis, noting the lower hysteresis of mesoporous coatings in comparison to dense coatings and implying benefits in moisture release. Findings underscore the need for a nuanced understanding of coating characteristics and their impact on sorption. In order to better assess the relationship between the coating content of the papers and their specific sorption properties, further investigations, such as the measurement of specific surface properties (e.g., specific surface area), are required. The findings of the water vapor diffusion resistance measurement study demonstrate a correlation between the observed resistance and the vapor levels. The results show that the water vapor diffusion resistance is elevated at lower vapor levels when compared to higher levels. This particular material behavior is typically employed within the construction industry for the utilization of moisture-variable water vapor retarders. The silica-paper hybrids exhibit a response that indicates the potential for advancement into a moisture-variable water vapor barrier.
Journal articles
Fast evaluation of spatial coating layer formation using ultraviolet scanner imaging
Fast evaluation of spatial coating layer formation using ultraviolet scanner imaging, TAPPI JOURNAL August 2015
Journal articles
A targeted approach to produce energy-efficient packaging materials from high-yield pulp, TAPPI Journal August 2025
ABSTRACT: Unlike fossil-based plastics, wood-based packaging materials can be produced in an ecofriendly manner using wood chip residuals from sawmills and pulpwood. To produce high-yield pulp like chemithermomechanical pulps (CTMPs) for paperboard and liquid packaging, it is crucial to reduce the electric energy consumption during fiber separation. The ultimate objective is to revolutionize paperboard production by achieving a middle-layer CTMP process that consumes less than 200 kilowatt-hours per metric ton (kWh/t), significantly improving from the current 500•600 kWh/t energy demand. Optimizing the CTMP impregnation process of sodium sulfite (Na2SO3) in wood chips is crucial for achieving uniform softening, ideally at the fiber level. The properties of the fibers are significantly affected by the content of lignin sulfonates within the walls of the fiber and the middle lamellae. In this study, we employed in-house developed X-ray fluorescence (XRF) techniques, validated by beamline measurements, to map the distribution of sulfonated lignin within fibers. It also seemed possible to enhance the surface area of lignin-rich pulp fibers while losing minimal bulk by refining them with well-optimized low consistency (LC) refining. We aimed to achieve a highly efficient separation of coniferous wood fibers by co-optimizing the sulfonation and the temperature in the preheater and chip refiner. Additionally, we explored how lignin’s softening behavior and potential crosslinking influence subsequent unit operations, including pressing, peroxide bleaching, and drying, following the defibration process. In defibration during chip refining, the maximum softening of wood fibers is preferred to maximize fiber preservation and minimize energy consumption. However, optimizing the stiffness of finished pulp fibers is preferable to reduce bulk loss during paperboard production. It can strive to optimize processes to develop stronger, lighter, and more sustainable composite packaging materials. Reducing environmental impact and electric energy can help create a more sustainable future.
Journal articles
Conversion of paper-grade pulp from rice straw into dissolving pulp, TAPPI Journal June 2025
ABSTRACT: About 1,165 million metric tons of rice straw is generated every year worldwide, which can be a good source for the circular bioeconomy. In this research paper, the paper-grade pulp from rice straw was converted to dissolving-grade pulp by fractionation in a biorefinery initiative. Rice straw was cooked at an optimum condition of 8% potassium hydroxide (KOH) charge for 120 min at 150°C and produced a pulp yield of 47.2% with a kappa number of 18.5. Subsequently, D0(EP)D1 bleaching was carried out for the produced pulp, and the brightness of the pulp reached to 82.4%. From the black liquor, 16.5% of the lignin and 11.9% of the hemicellulose were isolated for producing biobased products and chemicals, and then the spent liquor was used for soil amendment. The bleached pulp was fractionated in a Bauer McNett fiber classifier. The pulp fibers retained on 16-, 30-, and 50-mesh screens were used as a longer fiber fraction pulp, and pulp fibers retained on 100- and 200-mesh screens were used as a shorter fiber pulp. The longer and shorter fiber fraction pulps were analyzed for cellulose, R10, pentosan, and viscosity. The long fiber fraction pulps were characterized by higher cellulose (88.2% vs. 83.1%) and lower pentosan (11.3% vs. 13.0%) content than the shorter fiber fraction pulps. The longer fiber fraction was further treated with cold KOH to remove residual hemicellulose. The KOH extraction reduced pentosan content in pulp to 6.3% and increased á-cellulose content to 91.3%. The short fiber fraction was converted to monomeric sugars using cellulase enzymes with varying reaction time, temperature, and consistency. The efficiency of cellulase activity was assessed through glucose yield and residual dry weight. A temperature of 45°C, 5.0 pH, 5% consistency, and 6 filter paper units/gram (FPU/g) o.d. pulp resulted in maximum sugar conversion of 85.7%.
Journal articles
Paper strength factors in systems with nanofibrillated cellulose, cationic starch, colloidal silica, cationic acrylamide copolymer, and hydrodynamic shear, TAPPI Journal May 2025
ABSTRACT: Laboratory paper sheets were formed by first pretreating nanofibrillated cellulose (NFC) with cationic starch at the 5% level by mass. The treated NFC was then added to stock prepared from 100% recycled copy paper. The combined furnish was next optionally treated with a cationic retention aid (cPAM, 0.1%) and then colloidal silica (0.1% or 0.2%). Vacuum dewatering, fine-particle retention, and several paper properties were studied as a function of the colloidal silica level (zero, 1%, and 2%) and at different levels of shear stress applied just before forming the sheets. Dewatering and strength results were generally more favorable when using a medium charge cationic starch (~ 0.03 degree of substitution, DS) to pretreat the NFC rather than a high charge density cationic starch (~ 0.2 DS). In each case, the dewatering was further enhanced by subsequent treatments by cPAM (0.1% on whole furnish solids) and then even more with the final addition of colloidal silica (0.1% and 0.2% levels compared). However, the colloidal silica additions progressively hurt the tensile strength of the paper, especially in the case of the high charge cationic starch and at the higher level of colloidal silica. Though the dewatering performance was favorable, in such cases, the paper strength was not improved compared to paper made without any NFC. The fact that the systems involving cPAM treatment, and especially those involving both cPAM and colloidal silica, tended to reduce the resulting paper’s tensile strength supports a mechanism in which the additives result in the clustering of the NFC, possibly in multiparticle bunches. Evidence suggests that such bunches of clustered NFC particles, which are difficult to redisperse even at levels of hydrodynamic shear present in high-speed paper machine systems, are resistant to full integration into the sheet structure as the paper is being formed.
Journal articles
Magazine articles
Preparing prehydrolyzed kraft dissolving pulp via phosphotungstic acid prehydrolysis from grape branches, TAPPI Journal January 2022
ABSTRACT: Dissolving pulp was successful prepared via phosphotungstic acid (PTA) prehydrolysis kraft (PHK) cooking followed by an elementary chlorine-free (ECF) bleaching process from grape branches. The effects of prehydrolysis temperature, reaction time, and PTA concentration that potentially affect the quality of dissolving pulp product on chemical components of pulp were studied via an orthogonal experiment. The structure of lignin was activated during the PTA prehydrolysis phase, and lignin was easily removed during the following cooking process. Thus, relatively mild conditions (140°C, 100 min) can be used in the cooking process. During the prehydrolysis phase, temperature exhibited the most significant influence on the cellulose purity of the obtained pulp fiber, followed by reaction time and PTA concentration. The optimized prehydrolysis conditions were as follows: prehydrolysis temperature, 145°C; reaction time, 75 min; and PTA concentration, 1 wt%. Whether the excessively high prehydrolysis temperature or prolonging the reaction time did not favor the retention of long chain cellulose, the delignification selectivity for the cooking process could not be further improved by excessive PTA loading. Under these prehydrolysis conditions, 94.1% and 29.0% for a-cellulose content and total yield could be achieved after the given cooking and bleaching conditions, respectively. Moreover, the chemical structure and crystal form of cellulose were scarcely changed after PTA prehydrolysis, which could be confirmed by results from Fourier transform infrared (FTIR) spectroscopy and X-ray diffraction (XRD). PTA prehydrolysis could be considered as an alternative method for preparing PHK dissolving pulp under relatively mild cooking conditions.