Open Access
A new method of studying the fundamental mechanisms involved in pigment liberation from recycle papers, TAPPI Journal October 2022

ABSTRACT: Deinking flotation is the most efficient and widely used method of removing ink particles from printed papers to improve the recyclability. A prerequisite for successful deinking flotation is detachment of pigments from paper fibers, a subprocess known as liberation. The degree of liberation is usually determined via hyperwashing tests, which are costly and time consuming. Furthermore, they provide no information on the fundamental mechanisms controlling liberation. In the present work, we developed a new method in which ?-potentials of the particles in a pulp are measured and analyzed. If pigments are not liberated from paper fibers, a frequency distribution plot gives a single peak, while two peaks appear when they are liberated. One can readily determine the degrees of liberation from the peak positions and peak heights. In addition, the ?-potential data can be used to construct disjoining pressure isotherms using the DLVO theory that are useful to better understand the fundamental mechanisms involved and the roles of different reagents used to improve pigment liberation.

Open Access
Development of paper quality parameter measurement in China, TAPPI Journal May 2022

ABSTRACT: Paper quality parameters are important indicators of paper production, such as paper moisture, basis weight, ash content, strength, and so on. This study focuses on the online measurement methods and development of paper basis weight, moisture, and ash measuring. First, the measurable paper parameters and quality control system products in China are analyzed. Then, the basis weight measurement methods, accuracy, and development are given in the range of 10~1000 g/m2. Third, the distinction between infrared and microwave methods for moisture measurement is discussed. Finally, the ash measurement is introduced. Production and consumption of tissue paper in China have continually increased during the past decade. Near-infrared light technology is mature for the measurement of paper parameters in the range of 10~200 g/m2 basis weight. However, the near-infrared online measurement of tissue paper is not widely used, and few tissue paper lines are equipped with this type of quality control system in China. Therefore, technology for near-infrared measurement of basis weight has a great potential market in the field of tissue paper production. This article analyzes the future development trend of near-infrared light in tissue paper basis weight measurement and summarizes the difficulties in near-infrared light measurement of tissue paper basis weight.

Journal articles
Magazine articles
Open Access
Preparing prehydrolyzed kraft dissolving pulp via phosphotungstic acid prehydrolysis from grape branches, TAPPI Journal January 2022

ABSTRACT: Dissolving pulp was successful prepared via phosphotungstic acid (PTA) prehydrolysis kraft (PHK) cooking followed by an elementary chlorine-free (ECF) bleaching process from grape branches. The effects of prehydrolysis temperature, reaction time, and PTA concentration that potentially affect the quality of dissolving pulp product on chemical components of pulp were studied via an orthogonal experiment. The structure of lignin was activated during the PTA prehydrolysis phase, and lignin was easily removed during the following cooking process. Thus, relatively mild conditions (140°C, 100 min) can be used in the cooking process. During the prehydrolysis phase, temperature exhibited the most significant influence on the cellulose purity of the obtained pulp fiber, followed by reaction time and PTA concentration. The optimized prehydrolysis conditions were as follows: prehydrolysis temperature, 145°C; reaction time, 75 min; and PTA concentration, 1 wt%. Whether the excessively high prehydrolysis temperature or prolonging the reaction time did not favor the retention of long chain cellulose, the delignification selectivity for the cooking process could not be further improved by excessive PTA loading. Under these prehydrolysis conditions, 94.1% and 29.0% for a-cellulose content and total yield could be achieved after the given cooking and bleaching conditions, respectively. Moreover, the chemical structure and crystal form of cellulose were scarcely changed after PTA prehydrolysis, which could be confirmed by results from Fourier transform infrared (FTIR) spectroscopy and X-ray diffraction (XRD). PTA prehydrolysis could be considered as an alternative method for preparing PHK dissolving pulp under relatively mild cooking conditions.

Journal articles
Magazine articles
Open Access
Application of spruce wood flour as a cellulosic-based wood additive for recycled paper applications— A pilot paper machine study, TAPPI Journal October 2021

ABSTRACT: This study gives a first insight into the use of wood flour as a plant-based and cellulosic-based alter-native additive for newsprint and paperboard production using 100% recycled fibers as a raw material. The study compares four varieties of a spruce wood flour product serving as cellulosic-based additives at addition rates of 2%, 4%, and 6% during operation of a 12-in. laboratory pilot paper machine. Strength properties of the produced news-print and linerboard products were analyzed. Results suggested that spruce wood flour as a cellulosic-based additive represents a promising approach for improving physical properties of paper and linerboard products made from 100% recycled fiber content. This study shows that wood flour pretreated with a plant-based polysaccharide and untreated spruce wood flour product with a particle size range of 20 μm to 40 μm and 40 μm to 70 μm can increase the bulk and tensile properties in newsprint and linerboard applications.

Journal articles
Magazine articles
Open Access
Corrosion damage and in-service inspection of retractable sootblower lances in recovery boilers, TAPPI Journal October 2021

ABSTRACT: Several reports of accidents involving serious mechanical failures of sootblower lances in chemical recovery boilers are known in the pulp and paper industry. These accidents mainly consisted of detachment and ejection of the lance tip, or even of the entire lance, to the inside of the furnace, towards the opposite wall. At least one of these cases known to the author resulted in a smelt-water explosion in the boiler.In other events, appreciable damage or near-miss conditions have already been experienced. The risk of catastrophic consequences of the eventual detachment of the lance tip or the complete lance of a recovery boiler soot-blower has caught the attention of manufacturers, who have adjusted their quality procedures, but this risk also needs to be carefully considered by the technical staff at pulp mills and in industry committees.This paper briefly describes the failure mechanisms that prevailed in past accidents, while recommending inspection and quality control policies to be applied in order to prevent further occurrences of these dangerous and costly component failures. Digital radiography, in conjunction with other well known inspection techniques, appears to be an effective means to ensure the integrity of sootblower lances in chemical recovery boilers used in the pulp and paper industry.

Journal articles
Open Access
Corrosion Monitoring and Root Cause Identification in High Solids Concentrators

Black liquor high solids (about 80%) concentrators have often been found to suffer from aggressive corrosion. In particular, the first and second effect bodies are susceptible to corrosion attacks resulting in tube leaks and wall thinning, which limit the availability and lifetime of evaporator lines. Corrosion dynamics and construction materials have been studied extensively within the pulp and paper industry to understand the corrosion process. However, it has been challenging to identify root causes for corrosion, which has limited proactive measures to minimize corrosion damage. Corrosion of the first phase concentrator was studied by defining the potential regions for passive area, stress corrosion cracking, pitting corrosion, and general corrosion. This was achieved by using a technique called polarization scan that reveals ranges for the passive area in which the equipment is naturally protected against corrosion. The open circuit potential, also known as corrosion potential, and linear polarization resistance of the metal were monitored online, which allowed for definition of corrosion risks for stainless steel 304L and duplex stainless steels 2205 and SAF 2906. An online temperature measurement added insight to the analysis. A process diagnostics tool was used to identify root causes of the corrosion attacks. Many of the root causes were related to process conditions triggering corrosion. Once the metal surface was activated, it was difficult to repassivate the metal naturally unless a sufficient potential range was reached.

Journal articles
Magazine articles
Open Access
Evaluation of the particle size of organosolv lignin in the

Evaluation of the particle size of organosolv lignin in the synthesis of resol resins for plywood and their performance on fire spreading, TAPPI JOURNAL July 2017

Journal articles
Magazine articles
Open Access
Addition of corn stover arabinoxylan into hardwood during pu

Addition of corn stover arabinoxylan into hardwood during pulping for improved physical properties, TAPPI JOURNAL September 2017

Journal articles
Magazine articles
Open Access
The use of minerals in fiber-based packaging and pulp molding, TAPPI Journal January 2024

ABSTRACT: Minerals are widely used in the pulp and paper industry for aiding the processing, economics, and final quality of fiber-based products. Among these, calcium carbonate, talc, and kaolin are widely used as fillers, and these can have varying brightness, particle size distributions, and aspect ratios. For the molded fiber area, these minerals can raise the solids content of the pulp mixture and improve throughput and lower energy requirements for drying. Talc is also widely used as a process control agent, picking up pitch and stickies and improving productivity by lowering machine cleaning time.The replacement of single use plastic with fiber-based replacements is a global trend; however, it does come with some significant challenges, such as grease and moisture proofing. Previously, per- and polyfluoroalkyl substances (PFAS) have been used to provide functions such as water and grease repellency, but regulatory demands have seen its demise in the packaging industry. Therefore, water holdout is now generally achieved by addition of alkyl ketene dimer (AKD) sizing. Wax additives are being developed and tested as PFAS replacements for oil and grease resistance. Rather than strongly repelling lipids from the fiber surface, these PFAS alternatives restrict flow pathways and react with food oils to alter their flow characteristics to prevent penetration through the substrate. During studies incorporating both PFAS substitutes and minerals, no detrimental interactions were observed. This paper addresses the different needs of the molded fiber market by including mineral fillers in molded fiber articles and will be presented as a series of different case studies. In all studies, we show that the trends observed when mineral filler is added to molded fiber are broadly similar to those seen in conventional paper and paperboard applications. Mineral addition in all studies gave improvements in productivity and optical appearance. With its organophilic surface, hydrophobic talc had the additional advantage of pitch and sticky control, and although a small decrease in strength was always observed when filler was added, the final articles still retained sufficient strength for their particular application. This small strength reduction should be balanced against the productivity gains.

Journal articles
Magazine articles
Open Access
Experimental investigations into fold cracking of double coated barrier dispersion coatings, TAPPI Journal November 2024

ABSTRACT: The trend for replacing single-use plastics with fiber-based barrier coated board packaging has prompted a significant amount of research. There are many proposed ways of providing suitable packaging for applications like food service. Among these are dispersion coated barriers on board, as well as laminated boards that can be produced using conventional polyethylene (PE) or new biodegradable plastics. Minerals have also been shown to be suitable additives to these coatings for improving barrier performance through surface chemistry and by increasing the tortuosity of the pathway through the barrier layer. They also improve the cost effectiveness of the layer by lowering the material cost and raising the solids content, and by improving hold out of the functional layers, leading to a reduction in the amount of barrier coating needed to meet a given performance requirement. Minerals can also aid in the barrier handling in terms of rheology and reduced “stickiness,” as well as blocking of the films. When incorporated as fillers into extruded films, improved adhesion of the film to the board has been reported. One of the remaining challenges is the potential for cracking at the fold during converting and the loss of barrier performance that this can lead to. In this work, we systematically looked at the impact of mineral type and level in a dispersion coating. We assessed the differences in performance resulting from different coating application methods for the precoat layer by looking at the cracking tendency and loss of barrier functionality after folding for both the precoat alone and the final double coated sheets. Barrier results include moisture vapor transmission rate (MVTR), viscous vegetable oil, and the fluid blue stain in industrial methylated spirits (IMS) and Cobb water absorption, both before and after folding.