Journal articles
Paper strength factors in systems with nanofibrillated cellulose, cationic starch, colloidal silica, cationic acrylamide copolymer, and hydrodynamic shear, TAPPI Journal May 2025
ABSTRACT: Laboratory paper sheets were formed by first pretreating nanofibrillated cellulose (NFC) with cationic starch at the 5% level by mass. The treated NFC was then added to stock prepared from 100% recycled copy paper. The combined furnish was next optionally treated with a cationic retention aid (cPAM, 0.1%) and then colloidal silica (0.1% or 0.2%). Vacuum dewatering, fine-particle retention, and several paper properties were studied as a function of the colloidal silica level (zero, 1%, and 2%) and at different levels of shear stress applied just before forming the sheets. Dewatering and strength results were generally more favorable when using a medium charge cationic starch (~ 0.03 degree of substitution, DS) to pretreat the NFC rather than a high charge density cationic starch (~ 0.2 DS). In each case, the dewatering was further enhanced by subsequent treatments by cPAM (0.1% on whole furnish solids) and then even more with the final addition of colloidal silica (0.1% and 0.2% levels compared). However, the colloidal silica additions progressively hurt the tensile strength of the paper, especially in the case of the high charge cationic starch and at the higher level of colloidal silica. Though the dewatering performance was favorable, in such cases, the paper strength was not improved compared to paper made without any NFC. The fact that the systems involving cPAM treatment, and especially those involving both cPAM and colloidal silica, tended to reduce the resulting paper’s tensile strength supports a mechanism in which the additives result in the clustering of the NFC, possibly in multiparticle bunches. Evidence suggests that such bunches of clustered NFC particles, which are difficult to redisperse even at levels of hydrodynamic shear present in high-speed paper machine systems, are resistant to full integration into the sheet structure as the paper is being formed.
Journal articles
ABSTRACT: Lignin’s potential as a source of sustainable aromatic compounds is significant, but its utilization is currently limited by its chemical reactivity. Chemical reactivity of lignin depends on the present functional groups, such as hydroxyl, metho
ABSTRACT: Lignin’s potential as a source of sustainable aromatic compounds is significant, but its utilization is currently limited by its chemical reactivity. Chemical reactivity of lignin depends on the present functional groups, such as hydroxyl, methoxy, and carbonyl groups. Therefore, in this study, multivariate analysis-based chemometric models have been developed for rapid determination of aliphatic hydroxyl (Alp-OH) and phenolic hydroxyl (Ph-OH) groups in lignin samples. Two chemometric models, principal component regression (PCR) and partial least squares regression (PLSR), were established with Fourier transform infrared spectroscopy (FTIR) spectral data of 28 lignin samples. Both the models were developed based on raw and pretreated spectroscopic data with Savitky-Golay (S-G) filtering and standard normal variate (SNV) and multiplicative scatter correction (MSC). The predictive performance of the PLSR model is better for predicting Alp-OH (R2 = 0.94%), syringyl-OH (R2 = 0.96%), guaiacyl-OH (R2 = 0.98%), p-hydroxyphenyl (R2 = 0.93%), and total Ph-OH groups (R2 = 0.97%) with the data pretreated by MSC. Finally, the predicted results of these parameters for three new samples for the developed models are found to be very close to the estimated values by NMR.
Journal articles
ABSTRACT: This study investigates the impact of pulp screening on oxygen delignification of high lignin content kraft pulps from spruce wood. An alternative process is proposed: terminating kraft cooking at higher kappa numbers and applying oxygen deligni
ABSTRACT: This study investigates the impact of pulp screening on oxygen delignification of high lignin content kraft pulps from spruce wood. An alternative process is proposed: terminating kraft cooking at higher kappa numbers and applying oxygen delignification directly to unscreened and non-defibrated pulp. The objective is to evaluate whether this non-standard approach can maintain delignification efficiency while improving yield and reducing energy input. The findings demonstrate that screening prior to oxygen delignification is not essential for effective lignin removal or pulp quality. Similar delignification degrees and ISO brightness levels were obtained after oxygen delignification, whether it was performed on screened or unscreened pulps. Notably, the delignification rate in the oxygen stage was the same for the non-standard procedure as for pulp from the standard procedure with the reject fractionremoved prior to the oxygen stage. No significant differences were seen in fiber morphology, brightness level, orbrightness stability. The amount of total fiber charges in pulps not screened before oxygen delignification was slightly higher than in screened pulps.
Journal articles
Exploratory study on how sub-ply fiber orientation affects t
ABSTRACT: The transition to 100% biobased packaging presents considerable challenges, particularly in the development of a petroleum-free barrier. Generally, biobased barriers exhibit lower flexibility compared to traditional barriers, thereby increasing the risk of cracking during the converting process. The present study examines the possibility of optimizing the substrate to reduce cracking in brittle barriers. Five three-ply composites were fabricated using commercial paperboard to enable a composite with different fiber orientation in the individual plies. The different orientations achieved varying mechanical properties, including strain-atbreak and folding resistance, with a ranking that is comparable to a standard multi-ply paperboard. The composites were subjected to creasing at five distinct depths to assess the area percent of barrier cracks across the crease bead. Micro-cracks appeared on the surface before larger coating cracks were registered. As expected, the area percent of barrier cracks increased significantly with greater creasing depths. The orientation of the bulky middle ply showed little difference in the cracking propensity. However, by replacing the stiffer bottom ply with a ply of lower stiffness, the cracking propensity was significantly reduced without a substantial loss in mechanical properties. Hence, these findings indicate that it is possible to reduce the cracks in the barrier by modifying the fiber orientation in the different plies.
Journal articles
Improving barrier performance of coated paper and paperboard
ABSTRACT: Market demand for barrier coated packaging paper and paperboard has been on a steady rise and is forecasted to further increase. As a result, there is a continued interest in improving barrier coating functionalities, which is currently an active area of investigation. In this work, a multi-layer approach was adopted that involved applying a biowax emulsion, latex, or a combination of biowax and latex top coating layer onto the kaolin/latex (20/80, 50/50, 65/35, or 70/30) precoated solid bleached sulfate (SBS) paperboard. Our main objective was to demonstrate the effect of these top coating layers on various barrier properties, especially water vapor transmission rate (WVTR) at high relative humidity (RH) and high temperature (90% RH; 38°C), known as tropical/jungle test conditions. While the top coat with latex and/or biowax showed dramatic improvement in both water resistance (Cobb) and WVTR, the biowax coating increased contact angle significantly compared to the latex top coat. Contact angle increased from about 65° for the latex top coat to as high as 96° for the biowax top coat. Generally, it is much more difficult to improve WVTR at the jungle conditions below 100 g/m2/day, even with the high aspect ratio platy pigment. However, using the coating strategies adopted in this study, we were able to achieve WVTR values notably below 50 g/m2/day at the tropical test conditions, as well as significant improvements in regard to fold crack barrier integrity at high kaolin clay usage.
Journal articles
Prediction of residual calcium carbonate (CaCO3) in the lime
ABSTRACT: In a kraft pulp mill, the rotary lime kiln is responsible for converting calcium carbonate (CaCO3) into calcium oxide (CaO) to be reused in the causticizing plant. An important parameter of the calcination efficiency and the product quality is the amount of CaCO3 not converted to CaO, commonly defined as residual carbonate. This parameter is usually determined through laboratory analysis, which introduces delays in process control and limits the ability to make timely operational adjustments. This work presents a predictive model that functions as a soft sensor for the residual carbonate in a lime kiln of a Brazilian kraft pulp mill. This model was able to estimate residual CaCO3 every 30 min using routinely measured online process variables, which is a considerable reduction from the 6-h average laboratory measurement. The correlation coefficient (r) between the model predictions and the mill values was 0.83, with a mean absolute error (MAE) of 0.33%. Considering the effect of the residence time throughout the lime kiln proved to be decisive in obtaining a satisfactory prediction result. After model validation, a variable importance analysis showed that the carbon monoxide (CO) concentration in the stack flue gas (in ppm), secondary air temperature (in oC), and fan speed (in %) were the most influential variables in predicting the residual carbonate content. Combined with commonly used operation expertise, this subset of variables can serve as additional information to achieve smoother lime kiln operation.
Journal articles
Black liquor spray properties in-furnace conditions for swirl cone nozzles, TAPPI Journal July 2026
ABSTRACT: Recovery boiler furnace operation is controlled for high chemical recovery, high steam production, and low emissions. Good control allows long runs with minimum cleaning without expensive shutdowns. An essential variable affecting boiler operation is black liquor spraying into the furnace. Poorly controlled black liquor spraying causes difficulties, e.g., in chemical recovery, fouling of heat transfer surfaces, and decreased energy production. A challenging measurement strategy with three different swirl cone nozzles . types A, C, and T . was carried out at a mill in the United States. Black liquor spray properties were measured under in-furnace conditions for flow rates of 2.0 L/s to 3.0 L/s. Three spraying temperatures of 119™‹C, 122™‹C, and 126™‹C, which were 2™‹C, 5™‹C, and 9™‹C above the boiling point (ƒ¢Te), were tested. These flow rates and temperatures are typical for industrial nozzle sizes with exit orifice sizes of 17 mm and 22 mm. An imaging method to measure droplet size in a highly challenging furnace environment was developed. Droplet volume median diameter (Dv50) for nozzles A, C, and T varied between 7 mm to 4 mm, 7 mm to 5 mm, and 8 mm to 6 mm, depending on the flow rate and temperature. The high number of droplets detected by the analysis program enabled data fitting into statistical correlations. The size and width parameters for the Rosin™]Rammer droplet size distribution function could be defined. The droplet size distribution was found to be surprisingly wide, probably because of swollen droplets. Spray velocity was measured in two locations, 5 cm from the nozzle and 1.8 m from the nozzle. Near the nozzle, the average velocity increased from 7.3 m/s to 13 m/s when the flow rate was increased from 2 L/s to 3 L/s. Increase of black liquor temperature increased spray velocity in most of the cases. At the distance of 1.8 m from the nozzle, average spray velocities varied between 4.0 m/s to 11 m/s, depending on nozzle geometry, flow rate, and temperature. The opening angles of the spray for nozzles A and C varied between 57™‹ to 78™‹. The opening angle of nozzle T with flow guide varied between 48™‹ to 56™‹. The highest penetration of the spray was estimated for nozzle T because of the narrow spray and large droplets.
Journal articles
Non-process elements in the lime cycle: New findings regarding NPE distribution and lime mud filterability, TAPPI Journal July 2026
ABSTRACT: Proper functioning of the recausticizing cycle is crucial for securing a stable white liquor supply for a pulp mill. Common runnability problems in the modern lime cycle, such as low filterability and poor dewatering of lime mud, high dead load, or ring formation in the lime kiln, are often caused by accumulation of non-process elements (NPEs). This project attempted to verify the traditional rules of thumb regarding the chemical behavior of NPEs: magnesium (Mg), aluminum (Al), silicon (Si), phosphorus (P), zinc (Zn), manganese (Mn), iron (Fe), copper (Cu), barium (Ba), cadmium (Cd), and lead (Pb) in the causticizing reaction, and to investigate the reasons behind poor lime mud filterability. First, a standardized method for measuring filterability of lime mud was developed. Next, a series of recausticizing experiments, followed by immediate filtration trials, was conducted using mill green liquors, laboratory-made synthetic green liquor, reburned lime/makeup mix, and extra NPE additions. It was found that sodium (Na), potassium (K), and sulfur (S) followed the liquid phase, as expected, while Mg, P, and Ba, but also Pb, Cu, and Cd, showed low solubility and accumulated in the lime mud. The Si and Al accumulated in the lime mud even though the soluble content in liquor was high, while the behavior of Mn, Fe, and Zn was more complex. Based on these results, tentative solubility limits for NPEs were suggested as a first estimate for the maximum possible concentrations of NPEs in mill white liquor. The causticization-filtration experiments revealed that overliming and high content of Mg in green liquor clearly led to lower filterability, but our addition of Si did not have such an effect. As differences in particle size and size distribution have a certain impact on the filtration resistance, the lime mud sedimentation behavior, combined with other characterization methods, might be used as an indication for the filterability. Finally, a list of recommendations for pulp mills was formulated that starts with establishing a comprehensive standard for a lime mud with good filterability. This standard can be used as a benchmark for comparison any time a lime cycle runnability problem is identified.
Journal articles
A targeted approach to produce energy-efficient packaging materials from high-yield pulp, TAPPI Journal August 2025
ABSTRACT: Unlike fossil-based plastics, wood-based packaging materials can be produced in an ecofriendly manner using wood chip residuals from sawmills and pulpwood. To produce high-yield pulp like chemithermomechanical pulps (CTMPs) for paperboard and liquid packaging, it is crucial to reduce the electric energy consumption during fiber separation. The ultimate objective is to revolutionize paperboard production by achieving a middle-layer CTMP process that consumes less than 200 kilowatt-hours per metric ton (kWh/t), significantly improving from the current 500•600 kWh/t energy demand. Optimizing the CTMP impregnation process of sodium sulfite (Na2SO3) in wood chips is crucial for achieving uniform softening, ideally at the fiber level. The properties of the fibers are significantly affected by the content of lignin sulfonates within the walls of the fiber and the middle lamellae. In this study, we employed in-house developed X-ray fluorescence (XRF) techniques, validated by beamline measurements, to map the distribution of sulfonated lignin within fibers. It also seemed possible to enhance the surface area of lignin-rich pulp fibers while losing minimal bulk by refining them with well-optimized low consistency (LC) refining. We aimed to achieve a highly efficient separation of coniferous wood fibers by co-optimizing the sulfonation and the temperature in the preheater and chip refiner. Additionally, we explored how lignin’s softening behavior and potential crosslinking influence subsequent unit operations, including pressing, peroxide bleaching, and drying, following the defibration process. In defibration during chip refining, the maximum softening of wood fibers is preferred to maximize fiber preservation and minimize energy consumption. However, optimizing the stiffness of finished pulp fibers is preferable to reduce bulk loss during paperboard production. It can strive to optimize processes to develop stronger, lighter, and more sustainable composite packaging materials. Reducing environmental impact and electric energy can help create a more sustainable future.
Journal articles
Conversion of paper-grade pulp from rice straw into dissolving pulp, TAPPI Journal June 2025
ABSTRACT: About 1,165 million metric tons of rice straw is generated every year worldwide, which can be a good source for the circular bioeconomy. In this research paper, the paper-grade pulp from rice straw was converted to dissolving-grade pulp by fractionation in a biorefinery initiative. Rice straw was cooked at an optimum condition of 8% potassium hydroxide (KOH) charge for 120 min at 150°C and produced a pulp yield of 47.2% with a kappa number of 18.5. Subsequently, D0(EP)D1 bleaching was carried out for the produced pulp, and the brightness of the pulp reached to 82.4%. From the black liquor, 16.5% of the lignin and 11.9% of the hemicellulose were isolated for producing biobased products and chemicals, and then the spent liquor was used for soil amendment. The bleached pulp was fractionated in a Bauer McNett fiber classifier. The pulp fibers retained on 16-, 30-, and 50-mesh screens were used as a longer fiber fraction pulp, and pulp fibers retained on 100- and 200-mesh screens were used as a shorter fiber pulp. The longer and shorter fiber fraction pulps were analyzed for cellulose, R10, pentosan, and viscosity. The long fiber fraction pulps were characterized by higher cellulose (88.2% vs. 83.1%) and lower pentosan (11.3% vs. 13.0%) content than the shorter fiber fraction pulps. The longer fiber fraction was further treated with cold KOH to remove residual hemicellulose. The KOH extraction reduced pentosan content in pulp to 6.3% and increased á-cellulose content to 91.3%. The short fiber fraction was converted to monomeric sugars using cellulase enzymes with varying reaction time, temperature, and consistency. The efficiency of cellulase activity was assessed through glucose yield and residual dry weight. A temperature of 45°C, 5.0 pH, 5% consistency, and 6 filter paper units/gram (FPU/g) o.d. pulp resulted in maximum sugar conversion of 85.7%.