Factors affecting phosphorus uptake/dissolution during slaking and causticizing, TAPPI Journal March 2024

ABSTRACT: Hydroxide is regenerated in the recovery cycle of kraft pulp mills by the addition of lime (CaO) to green liquor. Phosphate in green liquor can react with the lime during slaking/causticizing. Total titratable alkali (TTA), sulfidity, the concentration of phosphate in the green liquor, temperature, and the liming ratio were all variables explored in this work to determine their influence on phosphorus uptake and dissolution. Experiments were also run in which the lime was slaked before being added to the green liquor to separate reactions with phosphate during slaking and reactions that occur during causticizing. Both reburnt lime and technical grade CaO were used. The experiment results indicate that phosphorus primarily reacts with slaked lime (Ca(OH)2), and that the final concentration of phosphate in the white liquor at the end of slaking and causticizing is nearly independent of the initial concentration of phosphorus and only mildly dependent on the carbonate concentration in the green liquor. There do appear to be differences in the rate at which phosphate reacts with reburnt lime and technical grade CaO, though the reason for this was not determined.

Journal articles
Magazine articles
Open Access
Utilization of Areca leaf residues for sustainable production of greyboard, TAPPI Journal May 2024

ABSTRACT: This study primarily focused on the production of greyboard using waste materials from small scale industries, and specifically using Areca leaf waste fibers as a sustainable and environmentally friendly resource. Areca leaf waste fibers were employed as the primary raw material for greyboard manufacturing. The resulting greyboard exhibited commendable properties, including a tear index of 7.53 mN·m2/g, tensile index of 18.34·N·m/g (i.e., breaking length of 1870 m), burst factor of 9.24 (gf/cm2)/(g/m2) and stiffness factor of 33.1. This greyboard was created through a series of steps, including hydrothermal treatment of the material at 155°C and mechanical pulping refinement. The produced greyboard met the specifications outlined in the Indian Standard 2617 (1967) for greyboard. The key objective of this work was to leverage agricultural waste resources to develop a chemical-free greyboard, resulting in reduced waste disposal in open fields and a decrease in chemical usage within the greyboard manufacturing industry. Various characterization techniques, including field emission scanning electron microscopy (FE-SEM), attenuated total reflection•Fourier transform infrared (ATR-FTIR) analysis, and X-ray diffraction (XRD), were used to assess the fiber quality, including aspects such as functional groups, morphology, and crystallinity for the materials used in the manufacturing process.

Journal articles
Magazine articles
Open Access
Continuous digester process safety improvements • Stress corrosion cracking and overpressure protection lessons learned and opportunities, TAPPI Journal October 2024

ABSTRACT: Georgia-Pacific has recent experience with continuous digester stress corrosion cracking (SCC) repairs where the extent of SCC was more than previous spot inspections had predicted (one digester had anodic protection, one did not). This paper offers case studies of reviewed and improved digester inspections by use of “boat” samples to quantify the depth of cracking mechanism. Boat sample test data is used to support repair recommendations based on hardness testing. Georgia-Pacific also reviewed overpressure protection systems and corrected gaps found in these systems. These included updating to the latest original equipment manufacturer (OEM) designs and formalizing functional testing procedures and practices. This review of digester inspection, testing, and repairs since 2020 provides: (1) a basis for including a 3rd party corrosion expert to be a part of inspections; (2) removes the use of power-wire brushes; (3) enhances digester inspection with 100% phased-array ultrasonic testing to detect SCC; and (4) ensures overpressure protection design and testing is aligned with corporate needs and the site-specific challenges.

Journal articles
Magazine articles
Open Access
How to use total dissolved solids measurements to evaluate the performance of diffuser washers—A mill study, TAPPI Journal April 2020

ABSTRACT: Various types of pulp washing equipment are available. Each washing device has a unique mechanical construction, and the washing principle is often a combination of dilution, thickening, and displacement washing. In this work, the performance of the pressure diffuser washer is studied. In stepwise trials, the effect of the feed and discharge consistencies on the performance of the diffuser was studied. The effect of the downward velocity of the screen on the pressure diffuser’s washing efficiency was also studied. The measurement of total dissolved solids (TDS) by a process refractometer was used as a wash loss measurement unit and the refractometer’s results were used in the calculations of standardized Nordén efficiency (E10) values. The chemical oxygen demand (COD) and conductivity values were also measured and their results compared to the TDS results.The results indicated that feed consistency has a significant effect on the performance and effectiveness of the diffuser washers in the mill. It can also be stated that when the downward velocity of the screen is adjusted to too high a level, the washing efficiency of the pressure diffuser decreases. As a conclusion from the mill tests, it can be stated that even small process parameter changes can provide enhanced diffuser washing at the beginning of the washing line, which has a direct effect on the performance of post-oxygen washing.

Journal articles
Magazine articles
Open Access
Mill experience of calcium carbonate scale formation in green liquor pipelines, TAPPI Journal August 2020

ABSTRACT: Experience of hard calcite (CaCO3) scale formation in green liquor pipelines at four kraft pulp mills was systematically investigated to determine if there is any correlation between the severity of the scaling problem at each mill and the design and operating conditions of its causticizing plant. The results show that the high degree of supersaturation of calcium ions (Ca2+) in the liquor is the main contributing factor. Mills that operate at a lower green liquor total titratable alkali (TTA), higher causticity, and a larger liquor temperature drop are more likely to produce a green liquor that is supersaturated with Ca2+, and thus experience more severe scaling problems. In order to minimize CaCO3 scaling, the green liquor handling equipment should be operated as steady as possible to avoid conditions that allow Ca2+ to be supersaturated. The strategies include minimizing variations in liquor TTA, insulating the green liquor pipelines to reduce temperature gradients, and adding lime mud to weak wash to provide seeds for precipitation to occur on mud particles instead of on metal substrate.

Journal articles
Magazine articles
Open Access
Kinetics of sulfur dioxide-alcohol-water (SAW) pulping of su

Kinetics of sulfur dioxide-alcohol-water (SAW) pulping of sugarcane straw (SCS), TAPPI JOURNAL June 2017

Journal articles
Magazine articles
Open Access
Pulping and bleaching of Malaysian oil palm empty fruit bunc

Pulping and bleaching of Malaysian oil palm empty fruit bunches, TAPPI JOURNAL June 2017

Journal articles
Magazine articles
Open Access
Lignin value prior to pulping (LVPP): An advanced pulping c

Lignin value prior to pulping (LVPP): An advanced pulping concept, TAPPI JOURNAL October 2017

Journal articles
Magazine articles
Open Access
Degradation of 2,4-dichlorophenol by melamine amine cellulos

Degradation of 2,4-dichlorophenol by melamine amine cellulose- immobilized lacasses, TAPPI JOURNAL October 2017

Journal articles
Magazine articles
Open Access
Combatting lime kiln ringing problems at the Arauco Constitución mill, TAPPI Journal July 2020

ABSTRACT: The lime kiln at the Arauco Constitución mill experienced severe ringing problems requiring it to be shut down for ring removal every 3 to 6 months. The mill controlled the problems by blasting ring deposits off during operation with its existing industrial shotgun and a newly installed Cardox liquid carbon dioxide (CO2) cartridge system. Various ring blasting procedures were tested to determine the optimum ring location and thickness to blast; the optimum depth to insert the CO2 cartridge into the kiln; and the most effective blasting frequency and sequence to employ. The best strategy was found to be the weekly blasting operation that alternated between the liquid CO2 cartridge and the industrial shotgun, with the CO2 cartridge inserted into the ring mass, 20 cm (8 in.) away from the refractory brick surface, and the shotgun aimed at rings at about 28 m (92 ft) from the kiln discharge end. With each blasting event removing considerably more rings than before, it takes a longer time for rings to rebuild, allowing the kiln to run continuously between annual maintenance shutdowns with only a few short (< 4 h) downtimes for ring removal. This substantially reduces the costs associated with ring removal and lime replacement during unscheduled shutdowns.