Search
Use the search bar or filters below to find any TAPPI product or publication.
Filters
Content Type
Publications
Level of Knowledge
Collections
Journal articles
Magazine articles
The Influence of the Fine Structure of Cellulose on the Action of Cellulases, TAPPI Journal June 2022
ABSTRACT: In the hydrolysis of cellulose with enzymes of Aspergillus niger at 47°C., it shown that a great decrease in the rate occurred in the late stage of the reaction, usually with considerable cellulose still reamaining undissolved.
Journal articles
Magazine articles
Boiler retrofit improves efficiency and increases biomass firing rates, TAPPI Journal March 2021
ABSTRACT: Domtar’s fluff pulp mill in Plymouth, NC, USA, operates two biomass/hog fuel fired boilers (HFBs). For energy consolidation and reliability improvement, Domtar wanted to decommission the No. 1 HFB and refurbish/retrofit the No. 2 HFB. The No. 2 HFB was designed to burn pulverized coal and/or biomass on a traveling grate. The steaming capacity was 500,000 lb/h from coal and 400,000 lb/h from biomass. However, it had never sustained this design biomass steaming rate. As the sole power boiler, the No. 2 HFB would need to sustain 400,000 lb/h of biomass steam during peak loads. An extensive evaluation by a combustion and boiler technologies supplier was undertaken. The evaluation involved field testing, analysis, and computational fluid dynamics (CFD) modeling, and it identified several bottle-necks and deficiencies to achieving the No. 2 HFB’s biomass steam goal. These bottlenecks included an inadequate combustion system; insufficient heat capture; excessive combustion air temperature; inadequate sweetwater con-denser (SWC) capacity; and limited induced draft fan capacity.To address the identified deficiencies, various upgrades were engineered and implemented. These upgrades included modern pneumatic fuel distributors; a modern sidewall, interlaced overfire air (OFA) system; a new, larger economizer; modified feedwater piping to increase SWC capacity; replacement of the scrubber with a dry electrostatic precipitator; and upgraded boiler controls.With the deployment of these upgrades, the No. 2 HFB achieved the targeted biomass steaming rate of 400,000 lb/h, along with lowered stack gas and combustion air temperatures. All mandated emissions limit tests at 500,000 lb/h of steam with 400,000 lb/h of biomass steam were passed, and Domtar reports a 10% reduction in fuel firing rates, which represents significant fuel savings. In addition, the mill was able to decommission the No. 1 HFB, which has substantially lowered operating and maintenance costs.
Journal articles
Magazine articles
Peracetate/singlet oxygen chemistry used in post-bleaching of kraft pulp as a practical oxidant for paper machines, TAPPI Journal May 2021
ABSTRACT: The use of a novel sodium peracetate/singlet oxygen chemistry for brightening bleached kraft pulp shows exciting potential for technical performance, supply logistics, safety, and cost reduction. Potential chemical carryover to the paper machine raises questions about whether peracetate will impact paper machine performance, such as metal corrosion, useful press felt life, and interference with existing biocide programs or paper machine chemistry. Sodium peracetate/singlet oxygen chemistry can be used in high-density storage chests for brightening/whitening and to increase color stability. Any oxidant used directly before the paper machine has the possibility of impacting paper machine operations. Traditional oxidants used in bleaching, such as chlorine dioxide and hydrogen peroxide, are known to cause corrosion on machinery metals and press felts. Hydrogen peroxide residuals can interfere with common biocide programs. Traditional oxidants used in biocide treatments themselves significantly degrade press felt life when the rule-of-thumb concentration thresholds are exceeded. Sodium peracetate is evaluated in this paper for its impact on nylon press felt fiber degradation, metal corrosion, and interference with typical biocide programs.Laboratory results indicate that sodium peracetate/singlet oxygen chemistry is less corrosive than chlorine, bromine, and hydrogen peroxide on press felt nylon fiber and can therefore be used at higher levels than those chemistries to increase brightness without increasing negative downstream impact. Sodium peracetate can also be used with current biocide programs without negative impacts such as consumptive degradation. Higher residuals of peracetate going to the paper machine may be useful as a biocide itself and can complement existing programs, allowing those programs to stay within their safe operating levels and thereby extend press felt useful life.
Journal articles
Magazine articles
Gas dispersion in the oxygen delignification process, TAPPI Journal May 2021
ABSTRACT: There has been very little knowledge about the state of gas dispersion in the oxygen delignification process, even though this has a major impact on the performance of the reactor. This paper presents a new continu-ous inline method for measuring oxygen bubble size distribution in the reactor, as well as results from studies con-ducted in softwood and hardwood lines. This new measurement worked well, and new information about oxygen bubble size, as well as how different reactor conditions affected the distribution, was obtained. For example:œ In the softwood line, the mean volume-weighted bubble size was about 0.1 mm, whereas in the hardwood line, this size was almost 10 times higher. For both lines, there was considerable variation in the measured bubble size over the long term.œ For both lines, an increase in mixer rotation speed caused a discernible decrease in the bubble size, and an increase in oxygen charge caused a discernible increase in the bubble size.œ In the softwood line, no coalescence of the bubbles in the reactor was observed, but in the hardwood line, some coalescence of the larger bubbles occurred.œ In the test conducted in the hardwood line, the use of brownstock washer defoamer caused a discernible increase in oxygen bubble size.œ In the hardwood line, reactor pressure had a noticeable effect on the amount of delignification, which indicated that improving mass transfer of oxygen (e.g., by decreasing the oxygen bubble size, in this case) should also have an increasing effect on the delignification.
Journal articles
Magazine articles
The role of gas dispersion in the oxygen delignification process, TAPPI Journal May 2021
ABSTRACT: Oxygen delignification is an essential part of the pulp production process. Delignification occurs with the aid of alkali and dissolved oxygen. Dissolved oxygen is obtained by dispersing oxygen gas into the pulp suspension by using efficient mixers. Little is known about the state of oxygen gas dispersion and its effect on oxygen delignification kinetics and efficiency. This paper will present the results for the effect of gas bubble size on the performance of oxygen delignification. The results are mainly based on detailed studies made in a Finnish hardwood mill where the oxygen bubble size distribution could be altered at the feed of the reactor. An essential aspect of these studies was the use of a new continuous inline gas bubble size measurement system to simultaneously determine the bubble size distribution at the feed and top of the reactor. Information about oxygen consumption in the reactor could also be obtained through the bubble size measurements. Accordingly, these studies quantify the effect of oxygen bubble size on the kappa reduction of the pulp. The effect of different chemical factors on the oxygen bubble size is also studied.Finally, the relationship between the gas bubble size and the liquid phase oxygen mass transfer coefficient (kLa) is presented. This connects the bubble size to the kappa reduction rate. Based on the presented modeling approach and the evaluation of practical factors that are not taken into account in the modeling, it was concluded that the volumetric average oxygen bubble size should preferably be smaller than 0.2 mm in practice.The information obtained with the new gas bubble size measurement system and the presented modeling approach give a very new basis for understanding, monitoring, adjusting, and designing oxygen delignification processes.
Journal articles
Magazine articles
Influence of pallet pattern on top-to-bottom compression performance of unitized loads, TAPPI Journal November 2021
ABSTRACT: Environmental scaling factors estimate a corrugated container’s ability to withstand various conditions it will encounter during the storage and distribution process. In this project, we examined the compressive resistance of unitized loads using differing pallet stacking patterns. To simulate real-world failure scenarios in our laboratory tests, we used two different nominal board grades of single-wall C-flute regular slotted containers loaded with a plywood panel and bagged salt to direct the failure location to the bottom of the stack. Our results showed that the columnar aligned pattern provided the greatest compressive resistance and the interlocked stacking arrangement yielded the lowest of the patterns evaluated. Based on the study results, we calculated box compression retention multipliers for each pattern and compared them to scaling factors published by the Fibre Box Association.
Journal articles
Magazine articles
Tetraethyl orthosilicate-containing dispersion coating — water vapor and liquid water barrier properties, TAPPI Journal September 2021
ABSTRACT: An aqueous styrene-butadiene latex dispersion coating containing in-situ processed tetraethyl orthosilicate (TEOS) applied on paperboard demonstrated improved water barrier performance. Coatings containing TEOS equivalent to 0.8% silicon dioxide (SiO2; dry basis) exhibited water vapor performance of < 25 g/m2/day (23°C, 50% relative humidity [RH]) and liquid water barrier performance Cobb 1800 s of < 6 g/m2, when applied as a single-layer 18 g/m2 coating. Cobb 1800 s barrier performance was still good (< 11 g/m2) at coat weights of 7•10 g/m2. The use of filler materials such as kaolin improved the vapor barrier properties of the coating, but this was not critical to the liquid water barrier properties.
Journal articles
Magazine articles
Commercially relevant water vapor barrier properties of high amylose starch acetates: Fact or fiction?, TAPPI Journal September 2021
ABSTRACT: Starches have recently regained attention as ecofriendly barrier materials due to the increased demand for sustainable packaging. They are easily processable by conventional plastics processing equipment and have been utilized for oil and grease barrier applications. While starches have excellent oxygen barrier properties and decent water barrier properties at low relative humidity (RH), they are moisture sensitive, as demonstrated by the deterioration of the barrier properties at higher RH values. Starch esters are chemically modified starches where the hydroxyl group of the starch has been substituted by other moieties such as acetates. This imparts hydrophobicity to starches and has been claimed as a good way of retaining water vapor barrier properties of starches, even at high RH conditions. We studied the water vapor barrier properties of one class of starch esters, i.e., high amylose starch acetates that were assumed to have good water vapor barrier properties. Our investigations found that with a high degree of substitution of hydroxyl groups, the modified starches did indeed show improvements in water vapor response as compared to pure high amylose starch films; however, the barrier properties were orders of magnitude lower than commercially used water vapor barriers like polyethylene. Even though these materials had improved water vapor barrier response, high amylose starch acetates are likely unsuitable as water vapor barriers by themselves, as implied by previous literature studies and patents.
Journal articles
Magazine articles
Orifice geometry as a tool for evaluating extensional flow resistance of barrier coating colors, TAPPI Journal November 2024
ABSTRACT: Knowledge of extensional flow behavior of coating colors can be beneficial for improving runnability and eliminating defects in various coating processes. The current work evaluates the use of an orifice geometry attached to a commercial capillary viscometer as a tool to obtain extensional flow properties of barrier coating dispersions. By measuring the pressure drop across the orifice as a function of flow velocity, the method presents the flow resistance as Euler number at industrially relevant high deformation rates. The results agree with the earlier results obtained with a capillary entrance pressure loss technique. The type of polymer additive is shown to control the extensional flow resistance, with high molecular weight linear flexible polymers such as polyethylene oxide (PEO) and polyvinyl alcohol (PVOH) having highest impact. The orifice method offers advantages over other approaches, including the need for only a small sample amount, ease of measurement, and access to high deformation rates.
Journal articles
Magazine articles
Experimental investigations into fold cracking of double coated barrier dispersion coatings, TAPPI Journal November 2024
ABSTRACT: The trend for replacing single-use plastics with fiber-based barrier coated board packaging has prompted a significant amount of research. There are many proposed ways of providing suitable packaging for applications like food service. Among these are dispersion coated barriers on board, as well as laminated boards that can be produced using conventional polyethylene (PE) or new biodegradable plastics. Minerals have also been shown to be suitable additives to these coatings for improving barrier performance through surface chemistry and by increasing the tortuosity of the pathway through the barrier layer. They also improve the cost effectiveness of the layer by lowering the material cost and raising the solids content, and by improving hold out of the functional layers, leading to a reduction in the amount of barrier coating needed to meet a given performance requirement. Minerals can also aid in the barrier handling in terms of rheology and reduced “stickiness,” as well as blocking of the films. When incorporated as fillers into extruded films, improved adhesion of the film to the board has been reported. One of the remaining challenges is the potential for cracking at the fold during converting and the loss of barrier performance that this can lead to. In this work, we systematically looked at the impact of mineral type and level in a dispersion coating. We assessed the differences in performance resulting from different coating application methods for the precoat layer by looking at the cracking tendency and loss of barrier functionality after folding for both the precoat alone and the final double coated sheets. Barrier results include moisture vapor transmission rate (MVTR), viscous vegetable oil, and the fluid blue stain in industrial methylated spirits (IMS) and Cobb water absorption, both before and after folding.