A new technique for the measurement of show-through mottle of fine paper, TAPPI Journal September 2019

ABSTRACT: Mottling within print-through and show-through is caused by the variability of the local optical properties of the sheet. This mottling is visually disturbing and a mark of poor paper quality. The ability to predict print-through mottle of printed paper by measuring show-through mottle on the unprinted sheet would be a valuable asset for paper machine control.We examined the relationship between print-through mottle and show-through mottle. We worked with nine samples of 60 lb. uncoated fine paper (90 g/m2), from various North American paper companies, that were printed on an offset press, 400K (400% Black), on both sides. A show-through mottle instrumental determination technique was developed using an existing Fast Fourier Transform-based algorithm. The nine samples examined were ranked similarly by the visual evaluation of print-through mottle and by the instrumental determination of show-through mottle. We thus established that show-through on the unprinted sheet can be used as a reliable predictor of print-through, therefore saving time and money for papermakers. We also found a significant two-sidedness in show-through for some of the samples.

Journal articles
Magazine articles
Open Access
Evaluation of folding effects on coating damage, TAPPI Journal November 2024

ABSTRACT: Barrier coatings on paperboard need to maintain integrity during converting and end-use for effective barrier performance. Folding is one of the most common deformations during converting; however, factors that affect damage during folding are not well defined. This is partly because methods to fold specimens and characterize damage are not standardized and the results are generally not transferable. In this work, we describe a method to fold paper specimens precisely and reproducibly. The keys to folding include using a defined geometry and controlled deformation. Multiple methods can be used to quantify damage; in this case, we use differences in permeability as a measure of how the coating becomes more open. Damage is sensitive to the degree of compression after the initial folding. Using a shim for support provides a defined amount of compression and minimizes the sensitivity to the applied pressure.

Journal articles
Magazine articles
Open Access
On increasing wet-web strength with adhesive polymers, TAPPI JOURNAL February 2020

ABSTRACT: Fiber-fiber adhesion, called “bonding” in the old paper physics literature, is a critical component of the overall strength of dry paper. With freshly formed very wet pulp fiber webs, all evidence suggests there are no fiber-fiber crossings with significant adhesive joint strength. With water removal, a point will be reached where fiber-fiber adhesion starts to contribute to the overall wet-web strength.The literature reveals very few examples of polymers that increase fiber-fiber joint strength in freshly formed webs. Here, we summarize the literature and explain why it is so difficult to promote fiber-fiber wet adhesion with polymers. Nevertheless, ongoing research in areas as diverse as tissue engineering scaffolds and biomimetic adhesives gives clues to future developments. Advances in paper machine engineering have lessened the importance of wet-web strength. By contrast, a critical issue in many of the evolving nanocellulose technologies is the strength of objects first formed by aqueous processing, the green strength—the strength of wet bodies before drying. For exam-ple, 3-D printed nanocellulose objects and ultralow density cellulosic aerogels can be destroyed by capillary forces during drying. There is a need for adhesives that strengthen freshly formed, wet lignocellulosic joints.

Journal articles
Magazine articles
Open Access
Effects of phosphogypsum whiskers modification with calcium stearate and their impacts on properties of bleached softwood paper sheets, TAPPI Journal September 2021

ABSTRACT: By combining the structural properties and characteristics of phosphogypsum whiskers, a preliminary study on the modification of phosphogypsum whiskers and their application in papermaking was carried out. The effects of reaction temperature, reaction time, and reaction concentration on the solubility and retention of modified phosphogypsum whiskers and the effects of phosphogypsum whiskers on the physical properties of paper under different modified conditions were explored. The research results show that, after the phosphogypsum whiskers are modified with calcium stearate, a coating layer will be formed on the surface of the whiskers, which effectively reduces the solubility of the phosphogypsum whiskers. The best modification conditions are: the amount of calcium stearate relative to the absolute dry mass of the phosphogypsum whisker is 2.00%; the modification time is 30 min, and the modification temperature is 60°C. The use of modified phosphogypsum whiskers for paper filling will slightly reduce the whiteness, folding resistance, burst resistance, and tensile strength of the paper, but the tearing degree and retention of the filler will be increased to some extent.

Journal articles
Magazine articles
Open Access
Three-dimensional pore structure visualization and character

Three-dimensional pore structure visualization and characterization of paper using X-ray computed tomography, TAPPI JOURNAL September 2017

Journal articles
Magazine articles
Open Access
Calender barring review with experiences, TAPPI Journal July 2022

ABSTRACT: Excessive calender vibration affects all styles of calender stacks from single to multi-nip, all hard rolls, or a combination of hard and soft rolls. Calender vibration can be forced vibration or self-excited vibration. Forced vibration occurs at the first few harmonics of the calender roll rotational speeds and is caused by imbalance, misalignment, eccentricity, etc. Self-excited vibration, the focus of this paper, occurs at higher frequencies. Feedback paths for self-excited vibration must be understood in order to ameliorate the problem. This is presented in the context of the historical development of the theory of self-excited feedback mechanisms, followed by a survey of self-excited feedback mechanisms in various types of calender stacks. Methodology to determine which feed-back path is present and techniques to control or eliminate the resulting vibration follow. To obtain a flavor of the types of problems faced and practical remedial actions, a variety of experiences with barring issues are provided.

Journal articles
Magazine articles
Open Access
Review of coating cracking and barrier integrity on paperboard substrates, TAPPI JournalDecember 2024

Authors: Joel C. Panek and Peter W. Hart | TAPPI J. 21(11): 589(2022) - ABSTRACT: Barrier packaging formats are major growth areas for the pulp and paper industry. It is technically challenging to maintain barrier properties during converting and end-use applications. Improved manufacturing capabilities and coating formulation knowledge will help maintain barrier integrity and enable growth of barrier products in challenging applications. These improvements will accelerate product development and commercialization, and allow faster response to product performance issues such as cracking. The literature on coating cracking provides knowledge mostly on the effects of coating formulations and to a lesser extent on substrate effects. Despite a large number of publications dedicated to coating failures, the approach to improve coating cracking remains empirical, and the transferability between studies and to real life applications has not been well established. Model development that successfully predicts commercial performance is in its infancy. However, some of these simplified models do a fairly good job predicting experimental data. The current work reviews the state of understanding as regards coating and barrier cracking and highlights the need for more research on cracking and barrier integrity.

Journal articles
Magazine articles
Open Access
Slot die coating of nanocellulose on paperboard, TAPPI Journal January 2018

Slot die coating of nanocellulose on paperboard, TAPPI Journal January 2018

Journal articles
Magazine articles
Open Access
On the nominal transverse shear strai to characterize the severity of creasing, TAPPI JOURNAL April 2018

On the nominal transverse shear strai to characterize the severity of creasing, TAPPI JOURNAL April 2018

Journal articles
Magazine articles
Open Access
Fundamental understanding of removal of liquid thin film trapped between fibers in the paper drying process: A microscopic approach, TAPPI Journal May 2020

ABSTRACT: In the fabrication of paper, a slurry with cellulose fibers and other matter is drained, pressed, and dried. The latter step requires considerable energy consumption. In the structure of wet paper, there are two different types of water: free water and bound water. Free water can be removed most effectively. However, removing bound water consumes a large portion of energy during the process. The focus of this paper is on the intermediate stage of the drying process, from free water toward bound water where the remaining free water is present on the surfaces of the fibers in the form of a liquid film. For simplicity, the drying process considered in this study corresponds to pure convective drying through the paper sheet. The physics of removing a thin liquid film trapped between fibers in the paper drying process is explored. The film is assumed to be incompressible, viscous, and subject to evaporation, thermocapillarity, and surface tension. By using a volume of fluid (VOF) model, the effect of the previously mentioned parameters on drying behavior of the thin film is investigated.