In-situ process monitoring in deep-drawing of paper using partially transparent tools, TAPPI Journal August 2025

ABSTRACT: The production of three-dimensionally formed packaging from paper by deep drawing usually leads to the occurrence of wrinkles, which result from the high tangential compressive stresses in the flange area and the limited flowability of the material. Wrinkles, although mostly tolerated in industry, end in both a reduced visual appearance and a reduction in usability for packaging, as with, for example, when gas-tightness is required. Previous research efforts have been limited to determining the wrinkle distribution after completion of forming and removal of the formed part. Consequently, the possibility of understanding the sequence of formation of individual wrinkles in the inhomogeneous material is lost. To remedy this situation, a method for local in-situ process monitoring is presented. Using a transparent die and an industrial camera, the flange area can be observed during the forming process. An image processing algorithm is applied to analyze the local development of the deep drawing process from the continuously recorded image data. The method described can be used to analyze the draw-in behavior and wrinkle formation locally and continuously over the drawing depth. The blank holder force influences the draw-in and the wrinkle pattern both locally and throughout the drawing process. A more precise understanding of the wrinkle formation will allow for more efficient process control in the future.

Journal articles
Controllable conversion of cellulose nanocrystals to cellulose microspheres: Insight on the effect of parameters during spray drying, TAPPI Journal February 2025

ABSTRACT: Cellulose microspheres, which have mainly been produced via the sol-gel method up until now, exhibit a promising potential for broad applications due to their regular microstructure and renewability. However, some issues with production of cellulose microspheres, such as the recycling of involved organic solvents and the removal of the residual solvents, should be solved. In this study, a cellulose nanocrystals (CNCs) suspension was used to produce cellulose microspheres via spray drying in order to avoid the use of organic solvents. The effects of CNCs particle size, CNCs concentration, and inlet temperature of spray drying on microstructure and particle size of cellulose microspheres were investigated. The results indicated that the optimal average particle size and concentration of CNCs used for obtaining cellulose microspheres were 106 nm and 0.1 wt%, respectively. Under the optimal conditions, cellulose microspheres with a regular spherical morphology and an average particle size of ca. 3 ìm were obtained. The sulfuric acid hydrolysis and spray drying process barely affected the crystalline structure of cellulose. However, the introduced sulfhydryl groups, which were confirmed by Fourier transform infrared spectroscopy results, degraded the thermostability of cellulose. Generally speaking, converting CNCs to cellulose microspheres via spray drying is beneficial for promoting the controllable and continuous production of cellulose microspheres.

Journal articles
The influence of precoating layers on the performance of water-based barrier coatings, TAPPI Journal January 2025

Cellulose nanofibrils (CNF) on paper have been demonstrated to be an effective barrier against oxygen and grease and have been shown to improve the barrier performance of dispersion-based barrier coatings. The potential to produce paper grades that have good oxygen, grease, and moisture barrier properties is clear, but a better understanding of the synergies between CNF, other coating layers, and water-based barrier coatings (WBBC) is needed to optimize these systems. Different coat weights of a commercial WBBC were applied to papers that have a range of different qualities and thicknesses of CNF precoating layers. The same WBBC was also applied to pigmented coated paper, with various types of pigments and latex levels. Samples were characterized in terms of grease resistance, water vapor transmission rate (WVTR), and oxygen transmission rate (OTR) before and after folding. The results were contrasted to cases where the WBBC was applied to the paper with no precoating layer. When the WBBC is applied on a CNF layer or the pigmented coating layer, the performance of the WBBC for the water vapor barrier improves a significant amount compared to when the WBBC is applied to the base paper with no precoating layer. This improvement likely comes from these precoating layers filling in the large paper pores, which leads to the WBBC forming a continuous layer at low coat weights. Folding decreases the moisture barrier performance to some degree, but the grease resistance is not influenced by folding when a CNF precoating layer is involved. Oxygen barrier properties are moderate for the CNF layer alone and are less than 5 cm3/m2/day when WBBC is coated on the CNF layer. This result likely comes from the barrier coating’s ability to repair defects in the CNF layer to stop the easy passage of oxygen in defect regions of the sample.

Journal articles
Open Access
Local delamination in pharmaceutical blister packages • A thermomechanical theory on buckling of heat-sealed composite laminates in flexible packaging, TAPPI Journal July 2025

ABSTRACT: Pharmaceutical blister packages consist of cavities made from a thick polymeric form foil and a thin aluminum lid foil. Heat-sealing technology is usually used to bond the lid foil to the form foil. Occasionally, the sealed area shows buckling defects of the lid foil, which allow contamination to enter into the cavity. A contaminated product is a worst-case scenario for pharmaceutical production and must be avoided. We discuss a thermomechanical theory on buckling defects in blister packages and derive strategies to avoid these. The theory is based on the assumption that the seal of a blister packaging behaves like a laminate of thin composite layers under compressive load. Literature research on buckling of thin laminated films, thermal behavior of polymers, and seal strength of heat-sealed polymers provides the technical and physical background to elaborate the theory. The theory comprises three elements: an initial condition regarding thermal load and precedent defects; a buckling condition; and a crack propagation condition. The plausibility of the theory is verified using model calculations and heat-seal tests. The paper concludes with strategies against buckling of heat-sealed lid foils and an outlook on other applications in laminating and coating of polymer films.

Journal articles
Open Access
Pilot-made, highly extensible paper for dry 3D forming, TAPPI Journal May 2025

Cellulose fiber-based packaging materials must perform well in demanding three dimensional (3D) forming process conditions. On the other hand, the development of manufacturing concepts is required for improved competitiveness of bio-based materials. This study covers some key factors that influence the extensibility of cellulose fiber-based structures and presents a pilot-scale development study of a 3D formable material concept. Bleached softwood kraft (BSK) pulp from a Nordic pulp mill was used in the pilot trials. Cellulose-based webs were formed using water-laid and foam-laid web forming using a pilot paper machine. For the water-laid forming, the BSK pulp was refined by applying a high consistency (HC) phase at over 40% consistency, followed by a low consistency (LC) refining at 4% consistency. The BSK pulp was refined for the foam-laid forming by only applying lowconsistency refining. In the foam-laid web forming, anionic sodium dodecyl sulfate (SDS), two foamable latexes, and polyvinyl alcohol (PVA) were used as foaming agents. The pilot rolls were dried at a separate steam cylinder dryer pilot and compacted in-plane in the machine direction (MD) at a separate pilot machine. Tensile properties of the treated paper webs were measured and evaluated with respect to achieved web shrinkage. The same dimensional contraction brought by shrinkage was almost strained out in tensile testing. The results indicated that the shrinkage that occurred by drying and in-plane compaction depended on the pulp furnish. The water-laid material achieved about 30% elongation, whereas the foam-laid material achieved significantly above 50% elongation. The 3D forming performance of the dry materials was tested using fixed and sliding blank methods. The dry paper sheets performed well enough in 3D forming for application to many consumer package applications according to their extensibility.

Journal articles
Magazine articles
Open Access
Peracetate/singlet oxygen chemistry used in post-bleaching of kraft pulp as a practical oxidant for paper machines, TAPPI Journal May 2021

ABSTRACT: The use of a novel sodium peracetate/singlet oxygen chemistry for brightening bleached kraft pulp shows exciting potential for technical performance, supply logistics, safety, and cost reduction. Potential chemical carryover to the paper machine raises questions about whether peracetate will impact paper machine performance, such as metal corrosion, useful press felt life, and interference with existing biocide programs or paper machine chemistry. Sodium peracetate/singlet oxygen chemistry can be used in high-density storage chests for brightening/whitening and to increase color stability. Any oxidant used directly before the paper machine has the possibility of impacting paper machine operations. Traditional oxidants used in bleaching, such as chlorine dioxide and hydrogen peroxide, are known to cause corrosion on machinery metals and press felts. Hydrogen peroxide residuals can interfere with common biocide programs. Traditional oxidants used in biocide treatments themselves significantly degrade press felt life when the rule-of-thumb concentration thresholds are exceeded. Sodium peracetate is evaluated in this paper for its impact on nylon press felt fiber degradation, metal corrosion, and interference with typical biocide programs.Laboratory results indicate that sodium peracetate/singlet oxygen chemistry is less corrosive than chlorine, bromine, and hydrogen peroxide on press felt nylon fiber and can therefore be used at higher levels than those chemistries to increase brightness without increasing negative downstream impact. Sodium peracetate can also be used with current biocide programs without negative impacts such as consumptive degradation. Higher residuals of peracetate going to the paper machine may be useful as a biocide itself and can complement existing programs, allowing those programs to stay within their safe operating levels and thereby extend press felt useful life.

Journal articles
Magazine articles
Open Access
Gas dispersion in the oxygen delignification process, TAPPI Journal May 2021

ABSTRACT: There has been very little knowledge about the state of gas dispersion in the oxygen delignification process, even though this has a major impact on the performance of the reactor. This paper presents a new continu-ous inline method for measuring oxygen bubble size distribution in the reactor, as well as results from studies con-ducted in softwood and hardwood lines. This new measurement worked well, and new information about oxygen bubble size, as well as how different reactor conditions affected the distribution, was obtained. For example:œ In the softwood line, the mean volume-weighted bubble size was about 0.1 mm, whereas in the hardwood line, this size was almost 10 times higher. For both lines, there was considerable variation in the measured bubble size over the long term.œ For both lines, an increase in mixer rotation speed caused a discernible decrease in the bubble size, and an increase in oxygen charge caused a discernible increase in the bubble size.œ In the softwood line, no coalescence of the bubbles in the reactor was observed, but in the hardwood line, some coalescence of the larger bubbles occurred.œ In the test conducted in the hardwood line, the use of brownstock washer defoamer caused a discernible increase in oxygen bubble size.œ In the hardwood line, reactor pressure had a noticeable effect on the amount of delignification, which indicated that improving mass transfer of oxygen (e.g., by decreasing the oxygen bubble size, in this case) should also have an increasing effect on the delignification.

Journal articles
Magazine articles
Open Access
The role of gas dispersion in the oxygen delignification process, TAPPI Journal May 2021

ABSTRACT: Oxygen delignification is an essential part of the pulp production process. Delignification occurs with the aid of alkali and dissolved oxygen. Dissolved oxygen is obtained by dispersing oxygen gas into the pulp suspension by using efficient mixers. Little is known about the state of oxygen gas dispersion and its effect on oxygen delignification kinetics and efficiency. This paper will present the results for the effect of gas bubble size on the performance of oxygen delignification. The results are mainly based on detailed studies made in a Finnish hardwood mill where the oxygen bubble size distribution could be altered at the feed of the reactor. An essential aspect of these studies was the use of a new continuous inline gas bubble size measurement system to simultaneously determine the bubble size distribution at the feed and top of the reactor. Information about oxygen consumption in the reactor could also be obtained through the bubble size measurements. Accordingly, these studies quantify the effect of oxygen bubble size on the kappa reduction of the pulp. The effect of different chemical factors on the oxygen bubble size is also studied.Finally, the relationship between the gas bubble size and the liquid phase oxygen mass transfer coefficient (kLa) is presented. This connects the bubble size to the kappa reduction rate. Based on the presented modeling approach and the evaluation of practical factors that are not taken into account in the modeling, it was concluded that the volumetric average oxygen bubble size should preferably be smaller than 0.2 mm in practice.The information obtained with the new gas bubble size measurement system and the presented modeling approach give a very new basis for understanding, monitoring, adjusting, and designing oxygen delignification processes.

Journal articles
Magazine articles
Open Access
A case study review of wood ash land application programs in North America, TAPPI Journal February 2021

ABSTRACT: Several regulatory agencies and universities have published guidelines addressing the use of wood ash as liming material for agricultural land and as a soil amendment and fertilizer. This paper summarizes the experiences collected from several forest products facility-sponsored agricultural application programs across North America. These case studies are characterized in terms of the quality of the wood ash involved in the agricultural application, approval requirements, recommended management practices, agricultural benefits of wood ash, and challenges confronted by ash generators and farmers during storage, handling, and land application of wood ash.Reported benefits associated with land-applying wood ash include increasing the pH of acidic soils, improving soil quality, and increasing crop yields. Farmers apply wood ash on their land because in addition to its liming value, it has been shown to effectively fertilize the soil while maintaining soil pH at a level that is optimal for plant growth. Given the content of calcium, potassium, and magnesium that wood ash supplies to the soil, wood ash also improves soil tilth. Wood ash has also proven to be a cost-effective alternative to agricultural lime, especially in rural areas where access to commercial agricultural lime is limited. Some of the challenges identified in the review of case studies include lengthy application approvals in some jurisdictions; weather-related issues associated with delivery, storage, and application of wood ash; maintaining consistent ash quality; inaccurate assessment of required ash testing; potential increased equipment maintenance; and misconceptions on the part of some farmers and government agencies regarding the effect and efficacy of wood ash on soil quality and crop productivity.

Journal articles
Magazine articles
Open Access
Key material properties in crease cracking of kraft paper, TAPPI Journal February 2021

ABSTRACT: Crease cracking of paperboard is important to control for the appearance and structural integrity of packages. Crease cracking is affected by creasing operation variables, as well as the physical properties of the paperboard. However, the effects of the physical properties are not clearly known. The objectives of this work were to identify the key material properties that affect crease cracking and to clarify the effects of fiber composition and starch. Laboratory sheets were produced from bleached and refined softwood and hardwood commercial pulp at grammage and thicknesses that match a typical paperboard. To mimic papermaking operations, surface starch was applied via a bench-top size press. The sheets were creased in the lab over a range of penetration depths, and reverse-side cracking was measured. The results showed that less reverse-side cracking was correlated with higher tensile post-peak energy, a lower bending stress, and a lower z-direction (ZD) stiffness. The tensile post-peak energy is a measure of the resistance to crack growth via fiber-bridging. The bending force and the ZD stiffness influence the forces that create cracks. It was observed that decreasing the ratio of hard-wood-to-softwood content and reducing the amount of starch would both decrease crease cracking.